How to hold ±0.01 mm on thin-wall aluminium parts
When a 1.5 mm wall springs back after unclamping, the machine is rarely the problem. Cutting forces deflect the wall while it is still supported, and residual stress redistributes once the fixture releases.
Three changes that work
First, reduce radial engagement and raise feed per tooth so the force vector pushes into the wall instead of bending it away. Second, rough and finish in separate passes with a stress-relief pause. Third, replace vice clamping with vacuum or low-pressure fixtures so the part is not pre-loaded.
Measure in the fixture
In-process probing before unclamping tells you whether the deviation comes from deflection or from thermal growth. On aluminium, a 4 °C shop swing over a long cycle is enough to move a 200 mm dimension by the full tolerance.
If you are designing a part with walls under 2 mm, send the model early. Adjusting the drawing is cheaper than chasing the tolerance in production.